Dear customers, Please kindly have an alert that according to our project experience, we foresee that many ICs will be in very tight supply or even out of stock for a long time, so please schedule your crucial projects of 2021 beforehand. : For more details, please have an alert to this news, down load Electronic Components Price Increase Reminder_Weller Technology Co., Limited

Panel plating

Panel plating after PTH process is to plate 5-8 um extra copper to the surface of PTH copper. This is to protect PTH copper from damage during the next following up process.

WELLER:
Copper thickness on through plated hole: 25um(min). Which is the same standard of IPC class 3.
Or else, the poor thickness copper on the through plated hole will take risk of open circuit after high temperature of assembly process.